An improved corrosion resistance is reached by the deposition of a proportional ratio CL-MP 308 nickel layer. The porosity of the chrome layer caused by CL-MP 308 is depending on the deposit thickness of the chrome layer. By 0.25 micrometre chrome are approx. 40.000 pores/cm achieved. By 0.50 micrometre approx. 20.000 pores/cm.

It is our pleasure to inform you in detail about our Microporous Nickel electrolyte.
Please contact us by phone (+49 (0) 212 658896-60) or by E-Mail info@cl-technology.de